    I was thinking (perhaps problems lies here), the Chinese 12k/15k stones - wouldn't they make decent nagura or slurry stones? Maybe even can be used to flatted stones post use?

    Start with DMT's and maybe finish with them? Is it possible/effective?



    TIA

  2. #2
    My opinion is that C12k stones, with or without slurry, are too hard and too slow for anything but razors.

  3. #3
    you can give it a try, no way of knowing without trying.
    I personally would not use it on a Jnat, because I think a Jnat slurry works differently and better, but still you will know if you like or not after giving it a try.

  4. #4
    Thanks guys
    I will definately try. Maybe it will work not to raise a slurry but to lap it. After a DMT, it will need something finer. awaiting my first JNS next week, so will try