hi KKF !
a small talk about "my" steel
as you know, i make my sanmaï myself. I use most of time the 145sc for the edge. and soft steel for the outside layers . this is not stainless.
the steel comp :
145sc :
the soft steel :
achim W, made another steel, 125sc, same as the 145sc but with "only" 1.25%c and more Mn, for oïl quenching .
the 144sc , is only for water quenching (or for thin thicknesses , with fast oïl like V35) .
a small talk about "my" steel
as you know, i make my sanmaï myself. I use most of time the 145sc for the edge. and soft steel for the outside layers . this is not stainless.
the steel comp :
145sc :
C 1,44%
Si 0,09
Mn 0,31
P 0,006
S 0,004
Cr < 0,1
Ni < 0,1
Mo < 0,1
Cu < 0,007
Al < 0,04
Ti < 0,001
Nb < 0,002
V < 0,004
W < 0,003
Co < 0,002
N < 0,003
Mg < 0,0003
As < 0,002
the soft steel :
C:0.03
Mn :0.2
P: 0.007
S: 0.002
Si: 0.20
Al: 0.042
Ni: 0.000
Nb: 0.000
V: 0.000
Cr: 0.000
Cu: 0.000
N: 0.007
Mo: 0.000
Ti: 0.000
Ceq : 0.000
B: 0.000
achim W, made another steel, 125sc, same as the 145sc but with "only" 1.25%c and more Mn, for oïl quenching .
the 144sc , is only for water quenching (or for thin thicknesses , with fast oïl like V35) .